Products

YAWATA 316L-16 (For 18%Cr-8%Ni-2%Mo)

Classification : AWS A 5.4 : E316L-16,  JIS Z 3221 : ES316L-16,  DIN 8556 : E 19 12 2 LR 26

Approvals :  ABS, TIS

Applications : Welding of all chromium-nickel steel with low or medium C content, as well as titamium and niobium stabilized chromium-nickel steel of 18%Cr-12%Ni-2%Mo type, e.g. material DIN No. 1.4401,1.4404, 1.4435, 1.4436, 1.4571, 1.4573, 1.4580, 1.4583, AISI 316, 316L, 318.

PDFYawata-Pamphlet-Stainless.pdf

 

YAWATA 316L-16 is a rutile high-alloy extra-low carbon electrode (ELC) for non-stabilized and stabilized chromium-nickel steels resistant to atmospheric corrosion of the 18%Cr-12%Ni-2%Mo type. Resistant to grain disintegration of operating temperatures up to 350℃. Smooth running, good striking and restriking. Regular appearance. Finely rippled, smooth junction, easy slag removal.

AWS A 5.4 : E316L-16
JIS Z 3211 : ES318L-16
DIN 8556 : E 19 12 2 LR 26
 
C
Si
Mn
P
S
Cr
Ni
Mo
Cu
Req.   
≤0.04
≤1.00
0.5-2.5
≤0.040
≤0.030
17.0-20.0
11.0-14.0
2.0-3.0
≤0.75
Typ.   
0.03
0.72
1.3
0.029
0.019
19.3
11.8
2.3
0.13
Req. = Requirement
Typ. = Typical results
N.S. = Not Specified
C.L. = Combined Limit for Mn + Ni + Cr + Mo + V
  Tensile Strength
N/mm2
(kgf/mm2)
Elongation
%
Charpy 2V-notch
J (kgf.m)
      at-20C at-40C
Req. ≥500 (51) 28 XXX XXX
Typ. 440 46 140 57
Diameter
/Length (mm)
2.0/250 2.6/300 3.2/350 4.0/350 5.0/350
Welding Position Current (A)
F 40-50 55-70 80-100 110-140 140-170
V, OH 35-45 45-65 70-90 100-130 -
1. Use dry electrodes only. Damp electrodes should be re-dried at 200~250℃ for 60 minutes before use.
2. Dirt such as oil, grease and dust should be completely removed from groove.
3. Excessively wide weaving may cause welding defects. Keep weaving width to less than 2.5 times electrodes diameter.