YAWATA 308L-16
(For Low Carbon 18%Cr-8%Ni Stainless Steel)

YAWATA 308L-16 now comes in small and economical-to-use size. The 4-piece vacuum pack will make sure that nothing goes to waste. It is a DIY favourite!!
 

Classification : AWS A 5.4 : E308L-16,  JIS Z 3221 : ES308L-16,  DIN 8556 : E 19 9 LR 26

Approvals : ABS, TIS

Application : Welding of all Cr-Ni steels with low or medium C content, as well as titamium and niobium stabilized Cr-Ni steels of the 18%Cr-8%Ni type, e.g. material DIN No 1.4300, 1.4301, 1.4306, 1.4541, 1.4543, 1.4550, AISI 302, 304, 304L, 321, 347.

PDFYawata-Pamphlet-Stainless.pdf

YAWATA 308L-16 is a rutile high-alloy extra-low carbon electrode (ELC) for non-stabilized and stabilized Cr-Ni steels resistant to atmospheric corrosion of the 18%Cr-8%Ni type. Re-sistant to grain disintegration of operating temperatures up to 350℃. Smooth running, good striking and restriking, regular appearance, finely rippled, smooth junction, easy slag removal.

AWS A 5.4 : E308L-16
JIS Z 3211 : ES308L-16
DIN 8556 : E 19 9 LR 26
 
C
Si
Mn
P
S
Cr
Ni
Mo
Cu
Req.    
≤0.04
≤1.00
0.5-2.5
≤0.040
≤0.030
18.0-21.0
9.0-11.0
≤0.75
≤0.75
Typ.    
0.03
0.80
1.1
0.028
0.018
20.1
9.3
0.14
0.13
Req. = Requirement
Typ. = Typical results
N.S. = Not Specified
C.L. = Combined Limit for Mn + Ni + Cr + Mo + V
  Tensile Stregth
N/mm(kgf/mm2)
Elongation
%
Creep-rupture strength
(as welded, 650ºC x 1000h

N/mm2)
Req.     ≥500(51) ≥28 ≥120
Typ.     500 (51) 28 120
Diameter
/Length (mm)
2.0/250 2.6/300 3.2/350 4.0/350 5.0/350
Welding Position Current (A)
F 40-50 55-70 80-100 110-140 140-170
V, OH 35-45 45-65 70-90 100-130 -
1. Use dry electrodes only. Damp electrodes should be re-dried at 200~250℃ for 60 minutes before use.
2. Dirt such as oil, grease and dust should be completely removed from groove.
3. Excessively wide weaving may cause welding defects. Keep weaving width to less than 2.5 times electrodes diameter.